  Effect of temperature on gold dissolution in acidic media

Cherevko, S., Žeradjanin, A. R., Topalov, A. A., Keeley, G. P., & Mayrhofer, K. J. J. (2014). Effect of temperature on gold dissolution in acidic media. Journal of the Electrochemical Society, 161(9), H501-H507. doi:10.1149/2.0551409jes.

Item is

Externe Referenzen

einblenden:

Urheber

einblenden:
ausblenden:
 Urheber:
Cherevko, Serhiy1, Autor           
Žeradjanin, Aleksandar R.1, Autor           
Topalov, Angel Angelov1, Autor           
Keeley, Gareth P.1, Autor           
Mayrhofer, Karl Johann Jakob1, Autor           
Affiliations:
1Electrocatalysis, Interface Chemistry and Surface Engineering, Max-Planck-Institut für Eisenforschung GmbH, Max Planck Society, ou_1863354              

Inhalt

einblenden:
ausblenden:
Schlagwörter: Arrhenius plots; Gold; Reaction intermediates; Apparent activation energy; Dissolution process; Effect of temperature; Galvanostatic polarization; Oxygen evolution reaction; Potentiodynamic experiments; Rate determining step; Temperature dependent
 Zusammenfassung: Temperature has a tremendous effect on the rate and amount of gold dissolution. In potentiodynamic experiments the total amount of dissolved gold increases by a factor of 4.5 when the temperature is increased from 25 to 75 degrees C. Moreover, the previously reported correlation between the onset of oxide formation and the commencement of the dissolution process is found to be correct for all studied temperatures. Negative shift in the advent of oxidation is accompanied by a similar shift in the dissolution onset potential. Similarly, the dissolution rate rises significantly with temperature during potentiostatic and galvanostatic polarization steps. A correlation between the temperature-dependent oxygen evolution reaction (OER) and gold dissolution is found. Arrhenius plots for the OER and gold dissolution are used to obtain information on the apparent activation energy EA for both processes. It is found that for OER and Au dissolution E-A = 57 kJ mol(-1). The later finding suggests that there is a common intermediate for both reactions, the formation of which constitutes the rate-determining step. (C) The Author(s) 2014. Published by ECS. This is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial No Derivatives 4.0 License (CC BY-NC-ND, http://creativecommons.org/licenses/by-nc-nd/4.0/), which permits non-commercial reuse, distribution, and reproduction in any medium, provided the original work is not changed in any way and is properly cited. For permission for commercial reuse, please email: oa@electrochem.org. All rights reserved.

Details

einblenden:
ausblenden:
Sprache(n): eng - English
 Datum: 2014
 Publikationsstatus: Erschienen
 Seiten: 7
 Ort, Verlag, Ausgabe: -
 Inhaltsverzeichnis: -
 Art der Begutachtung: Expertenbegutachtung
 Identifikatoren: ISI: 000340019600104
DOI: 10.1149/2.0551409jes
 Art des Abschluß: -

Veranstaltung

einblenden:

Entscheidung

einblenden:

Projektinformation

einblenden:

Quelle 1

einblenden:
ausblenden:
Titel: Journal of the Electrochemical Society
Genre der Quelle: Zeitschrift
 Urheber:
Affiliations:
Ort, Verlag, Ausgabe: New York, NY, USA : Electrochemical Society
Seiten: - Band / Heft: 161 (9) Artikelnummer: - Start- / Endseite: H501 - H507 Identifikator: ISSN: 0013-4651
CoNE: https://pure.mpg.de/cone/journals/resource/991042748197686