  Supersaturation of Iron with Nitrogen, Hydrogen or Carbon and the Consequences

Grabke, H. J. (2004). Supersaturation of Iron with Nitrogen, Hydrogen or Carbon and the Consequences. Materiali in Tehnologije, 38, 25-36.

Item is

Files

show Files

Locators

show

Creators

show
hide
 Creators:
Grabke, H. J.1, Author           
Affiliations:
1External Organizations, ou_persistent22              

Content

show

Details

show
hide
Language(s): eng - English
 Dates: 2004
 Publication Status: Issued
 Pages: -
 Publishing info: -
 Table of Contents: -
 Rev. Type: -
 Identifiers: eDoc: 204255
 Degree: -

Event

show

Legal Case

show

Project information

show

Source 1

show
hide
Title: Materiali in Tehnologije
Source Genre: Journal
 Creator(s):
Affiliations:
Publ. Info: -
Pages: - Volume / Issue: 38 Sequence Number: - Start / End Page: 25 - 36 Identifier: -