  The durability of polyol-synthesized PtRu/C for direct methanol fuel cells

Guo, J., Sun, G., Wu, Z., Sun, S., Yan, S., Cao, L., et al. (2007). The durability of polyol-synthesized PtRu/C for direct methanol fuel cells. Journal of Power Sources, 172(2), 666-675. Retrieved from http://dx.doi.org/10.1016/j.jpowsour.2007.05.012.

Item is

Dateien

einblenden: Dateien
ausblenden: Dateien
:
337750+Vorblatt.pdf (beliebiger Volltext), 3MB
 
Datei-Permalink:
-
Name:
337750+Vorblatt.pdf
Beschreibung:
-
OA-Status:
Sichtbarkeit:
Privat
MIME-Typ / Prüfsumme:
application/pdf
Technische Metadaten:
Copyright Datum:
-
Copyright Info:
-
Lizenz:
-

Externe Referenzen

einblenden:

Urheber

einblenden:
ausblenden:
 Urheber:
Guo, Junsong, Autor
Sun, Gongquan, Autor
Wu, Zhimou, Autor
Sun, Shiguo, Autor
Yan, Shiyou, Autor
Cao, Lei, Autor
Yan, Yushan, Autor
Su, Dangsheng1, Autor           
Xin, Qin, Autor
Affiliations:
1Inorganic Chemistry, Fritz Haber Institute, Max Planck Society, ou_24023              

Inhalt

einblenden:
ausblenden:
Schlagwörter: Direct methanol fuel cell; PtRu; Durability; Unalloyed Ru Carbon
 Zusammenfassung: The durability of polyol-synthesized PtRu/C as anode electrocatalyst for direct methanol fuel cells (DMFCs) has been studied by conducting a 2020-h life-test of a single cell discharging at a constant current density of 100mAcm−2. Critical fuel cell performance parameters including anode activity, cathode activity and internal resistance are, for the first time, systematically examined at the life-test time of 556, 1093, 1630 and 2020 h. High-resolution transmission electron microscopy and X-ray diffraction (XRD) have also been performed and show that PtRu nanoparticles have agglomerated with the mean particle size increasing from 1.82 to 2.78 nm after the 2020-h life-test. Anode polarization and electrochemical impedance spectroscopy (EIS) show that there exists a stable discharging period where the anode polarization potential is less than 0.363V versus dynamic hydrogen electrode (DHE). When the anode polarization potential exceeds 0.363V versus DHE, the performance of the anode degrades dramatically due to the leaching of the unalloyed Ru as indicated by energy dispersive X-ray spectroscopy (EDS) and XRD. This finding provides clues in developing strategies to operate fuel cells achieving maximum lifetime without noticeable performance lose.

Details

einblenden:
ausblenden:
Sprache(n): eng - English
 Datum: 2007
 Publikationsstatus: Erschienen
 Seiten: -
 Ort, Verlag, Ausgabe: -
 Inhaltsverzeichnis: -
 Art der Begutachtung: Expertenbegutachtung
 Identifikatoren: eDoc: 337750
URI: http://dx.doi.org/10.1016/j.jpowsour.2007.05.012
 Art des Abschluß: -

Veranstaltung

einblenden:

Entscheidung

einblenden:

Projektinformation

einblenden:

Quelle 1

einblenden:
ausblenden:
Titel: Journal of Power Sources
Genre der Quelle: Zeitschrift
 Urheber:
Affiliations:
Ort, Verlag, Ausgabe: -
Seiten: - Band / Heft: 172 (2) Artikelnummer: - Start- / Endseite: 666 - 675 Identifikator: -