  Rapid Genesis of Active Phase during Calcination of Promoted Sulfated Zirconia Catalysts

Hahn, A. H. P., Jentoft, R. E., Ressler, T., Weinberg, G., Schlögl, R., & Jentoft, F. C. (2005). Rapid Genesis of Active Phase during Calcination of Promoted Sulfated Zirconia Catalysts. Journal of Catalysis, 236, 324-334. doi:10.1016/j.jcat.2005.09.035.

Item is

Files

show Files
hide Files
:
hahn_jentoft_szcalcination_revisedfinal.pdf (Any fulltext), 616KB
Name:
hahn_jentoft_szcalcination_revisedfinal.pdf
Description:
-
OA-Status:
Visibility:
Public
MIME-Type / Checksum:
application/pdf / [MD5]
Technical Metadata:
Copyright Date:
-
Copyright Info:
-
License:
-
:
738529 CTA.pdf (Copyright transfer agreement), 93KB
 
File Permalink:
-
Name:
738529 CTA.pdf
Description:
-
OA-Status:
Visibility:
Private
MIME-Type / Checksum:
application/pdf
Technical Metadata:
Copyright Date:
-
Copyright Info:
-
License:
-
:
738529.pdf (Correspondence), 149KB
 
File Permalink:
-
Name:
738529.pdf
Description:
-
OA-Status:
Visibility:
Private
MIME-Type / Checksum:
application/pdf
Technical Metadata:
Copyright Date:
-
Copyright Info:
-
License:
-

Locators

show

Creators

show
hide
 Creators:
Hahn, Alexander H. P.1, Author           
Jentoft, Rolf E.1, Author           
Ressler, Thorsten1, Author           
Weinberg, Gisela1, Author           
Schlögl, Robert1, Author           
Jentoft, Friederike C.1, Author           
Affiliations:
1Inorganic Chemistry, Fritz Haber Institute, Max Planck Society, ou_24023              

Content

show
hide
Free keywords: promoted sulfated zirconia, iron, manganese, preparation, calcination, butane isomerization, morphology, in situ XRD Project 1: Acid-base & redox properties of promoted sulfated zirconia
 Abstract: Amorphous sulfated zirconium hydroxide was promoted with iron or manganese via the incipient wetness technique, to give 0.5–3.5 weight% promoter in the final catalyst. An exothermic reaction during the calcination temperature ramp (to 823 or 923 K) leads to a rapid overheating (“glow”) of the sample. XRD shows that crystallization starts before and progresses during the overheating. The surface area shrinks during the glow, and its final size (85–120 m2•g-1) and the porosity appear to be largely determined by the glow event. Manganese and iron ions prevent the coalescence of particles and lead to high surface areas. Variation of the batch volume (2.2, 8.4, or 17.1 ml) for calcination produced different catalysts from the same precursor. For both promoters, samples calcined in large batches exhibited the highest surface areas, interconnected mesopores (2.2–3.8 nm), and the highest maximum rate in n-butane isomerization (338 K, 1 kPa n-butane). Long term performance was independent of surface area and morphology. The concentration of the active sites depended on the calcination batch size, indicating that the active phase is formed in kinetically controlled reactions during the rapid overheating. The catalytic and textural properties of sulfated zirconia catalysts can be reproduced through controlling the batch size used for calcination.

Details

show
hide
Language(s): eng - English
 Dates: 2005-11-10
 Publication Status: Issued
 Pages: -
 Publishing info: -
 Table of Contents: -
 Rev. Type: Peer
 Identifiers: eDoc: 245298
DOI: 10.1016/j.jcat.2005.09.035
 Degree: -

Event

show

Legal Case

show

Project information

show

Source 1

show
hide
Title: Journal of Catalysis
  Alternative Title : J. Catal.
Source Genre: Journal
 Creator(s):
Affiliations:
Publ. Info: -
Pages: - Volume / Issue: 236 Sequence Number: - Start / End Page: 324 - 334 Identifier: -