Effects of charring on mass, organic carbon, and stable carbon isotope composition of wood

MPS-Authors
/persons/resource/persons62360

Czimczik,  C. I.
Department Biogeochemical Processes, Prof. E.-D. Schulze, Max Planck Institute for Biogeochemistry, Max Planck Society;

/persons/resource/persons62603

Werner,  R. A.
Service Facility Stable Isotope/Gas Analytics, Dr. W. A. Brand, Max Planck Institute for Biogeochemistry, Max Planck Society;

/persons/resource/persons62549

Schulze,  E.-D.
Department Biogeochemical Processes, Prof. E.-D. Schulze, Max Planck Institute for Biogeochemistry, Max Planck Society;

External Resource
There are no locators available
Fulltext (restricted access)
There are currently no full texts shared for your IP range.
フルテキスト (公開)
公開されているフルテキストはありません
付随資料 (公開)
There is no public supplementary material available
引用

Czimczik, C. I., Preston, C. M., Schmidt, M. W. I., Werner, R. A., & Schulze, E.-D. (2002). Effects of charring on mass, organic carbon, and stable carbon isotope composition of wood. Organic Geochemistry, 33(11), 1207-1223.


引用: https://hdl.handle.net/11858/00-001M-0000-000E-CED1-F
要旨
To aid in understanding black carbon (BC) formation during smoldering combustion in forest fires, we characterized charring of a softwood and hardwood. Charring (150, 340, 480 degreesC) caused mass loss (7-84%), enrichment of organic carbon (OC) (0-32%), and C-13 depletion (> 150 degreesC). As determined by C-13 MAS NMR, the OC composition of the woods was dominated by (di)-O-alkyl structures, and the chars by alkyl and aromatic structures. With increasing temperature, aromatic structures increased and the chars became more similar, although initial differences in OC concentration and delta(13)C of woods persisted. The BC cluster sizes apparently remained small, pointing towards a low resistance against oxidation. Crown Copyright (C) 2002 Published by Elsevier Science Ltd. All rights reserved.