English
 
Help Privacy Policy Disclaimer
  Advanced SearchBrowse

Item

ITEM ACTIONSEXPORT

Released

Journal Article

“Cubism” on the nanoscale : from squaric acid to porous carbon cubes

MPS-Authors
/persons/resource/persons192581

Mani,  Christian Mbaya
Nina Fechler, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

/persons/resource/persons192583

Berthold,  Thomas
Nina Fechler, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

/persons/resource/persons121280

Fechler,  Nina
Nina Fechler, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

External Resource
No external resources are shared
Fulltext (restricted access)
There are currently no full texts shared for your IP range.
Fulltext (public)

2265712_cover.pdf
(Publisher version), 7MB

Supplementary Material (public)
There is no public supplementary material available
Citation

Mani, C. M., Berthold, T., & Fechler, N. (2016). “Cubism” on the nanoscale: from squaric acid to porous carbon cubes. Small, 12(21), 2906-2912. doi:10.1002/smll.201600284.


Cite as: https://hdl.handle.net/11858/00-001M-0000-002A-33DE-7
Abstract
3D cube-shaped composites and carbon microparticles with hierarchically porous structure are prepared by a facile template-free synthesis route. Via the coordination of zinc acetate dihydrate and squaric acid, porous 3D cubic crystalline particles of zinc squarate can be obtained. These are easily transformed into the respective zinc oxide carbon composites under preservation of the macromorphology by heat treatment. Washing of the composite materials results in hierarchically porous carbons with high surface areas (1295 m2 g–1) and large pore volumes (1.5 cm3 g−1) under full retention of the cube-like architecture of the initial crystals. The materials are shown to be promising electrode materials for supercapacitor applications with a specific capacitance of 133 F g−1 in H2SO4 at a scan rate of 5 mV s−1, while 67 of this specific capacitance is retained, when increasing the scan rate to 200 mV s−1.