Structure and magnetic properties of (Cr,Ni)4-x CoxSi

MPS-Authors
/persons/resource/persons126852

Sichevych,  Olga
Chemical Metal Science, Max Planck Institute for Chemical Physics of Solids, Max Planck Society;

/persons/resource/persons126541

Borrmann,  Horst
Horst Borrmann, Chemical Metal Science, Max Planck Institute for Chemical Physics of Solids, Max Planck Society;

/persons/resource/persons146769

Bobnar,  Matej
Chemical Metal Science, Max Planck Institute for Chemical Physics of Solids, Max Planck Society;

/persons/resource/persons126510

Akselrud,  Lev
Chemical Metal Science, Max Planck Institute for Chemical Physics of Solids, Max Planck Society;

External Resource
No external resources are shared
Fulltext (restricted access)
There are currently no full texts shared for your IP range.
Fulltext (public)
There are no public fulltexts stored in PuRe
Supplementary Material (public)
There is no public supplementary material available
Citation

Martyniak, R.-I., Muts, N., Sichevych, O., Borrmann, H., Bobnar, M., Akselrud, L., et al. (2019). Structure and magnetic properties of (Cr,Ni)4-x CoxSi. Solid State Phenomena, 289, 108-113. doi:10.4028/www.scientific.net/SSP.289.108.


Cite as: https://hdl.handle.net/21.11116/0000-0004-88FE-5
Abstract
The crystal structure of the (Cr,Ni)4 Si phase with and without Co was refined from X-ray powder diffraction data. The compound crystallises with an Au4 Al-type structure (Pearson symbol cP20, space group P21 3): unit-cell parameter a = 0.611959(6) nm for the composition (Cr0.312 Ni0.688 )4 Si, a = 0.612094(6) nm for (Cr0.375 Ni0.625 )4Si, and a = 0.612316(6) nm for (Cr0.337 Co0.063 Ni0.600 )4Si. The magnetic susceptibility was measured in external fields up to 7 T at temperatures between 1.8 and 400 K. The three investigated samples exhibited paramagnetic behaviour described by the modified Curie-Weiss law: χ0 = 146∙10-6 emu g-at.-1, μeff = 0.21 μB /atom, θP =-13 K for (Cr0.312 Ni0.688 )4 Si; χ0 = 158∙10-6 emu g-at.-1, μeff = 0.20 μB /atom, θP =-15 K for (Cr0.375Ni0.625 )4Si; χ0 = 169∙10-6 emu g-at.-1, μeff = 0.18 μB/atom, θP =-52 K for (Cr0.337 Co0.063 Ni0.600 )4Si. © 2019 Trans Tech Publications, Switzerland.