Structural, photocatalytic and electroconductive properties of bismuth-substituted CaMoO4

MPS-Authors
/persons/resource/persons212917

Tarakina,  Nadezda V.
Nadezda V. Tarakina, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

/persons/resource/persons250334

Piankova,  Diana V.
Nadezda V. Tarakina, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

External Resource
No external resources are shared
Fulltext (restricted access)
There are currently no full texts shared for your IP range.
Fulltext (public)
There are no public fulltexts stored in PuRe
Supplementary Material (public)
There is no public supplementary material available
Citation

Mikhaylovskaya, Z. A., Abrahams, I., Petrova, S. A., Buyanova, E., Tarakina, N. V., Piankova, D. V., et al. (2020). Structural, photocatalytic and electroconductive properties of bismuth-substituted CaMoO4. Journal of Solid State Chemistry, 291: 121627. doi:10.1016/j.jssc.2020.121627.


Cite as: https://hdl.handle.net/21.11116/0000-0006-F223-1
Abstract
The Ca1−3xBi2xФxMoO4 system (0.025 ≤ x ≤ 0.30, where Ф represents cation vacancies) was synthesized and studied. The 0.025 = x ≤ 0.15 compositions show a tetragonal defect scheelite structure. Powder X-ray and neutron diffraction patterns for compositions with 0.15 < x ≤ 0.225 exhibit a tetragonal supercell with asup ≈ √5a, csup ≈ c where a and c are the tetragonal scheelite cell parameters. Transmission electron microscopy shows that Ca0.4Bi0.4MoO4, crystals consist of three crystallographic domains: (1) defect scheelite; (2) tetragonal superlattice and (3) incommensurately modulated. Photocatalytic properties were studied using Rhodamine B water solutions under UV light. Catalytic activity increases with increasing Bi content. The conductivity of 0.15 < x ≤ 0.225 compositions is 10−7 to 10−8 S cm−1 in the range 500–650 °C, while compositions in the range 0.025 = x ≤ 0.15 show conductivity values from 10−3 to 10−8 S cm−1 from 500 to 800 °C.