Deutsch
 
Hilfe Datenschutzhinweis Impressum
  DetailsucheBrowse

Datensatz

DATENSATZ AKTIONENEXPORT

Freigegeben

Zeitschriftenartikel

High-performance all-bio-based laminates derived from delignified wood

MPG-Autoren
/persons/resource/persons121298

Fratzl,  Peter
Peter Fratzl, Biomaterialien, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

Externe Ressourcen
Es sind keine externen Ressourcen hinterlegt
Volltexte (beschränkter Zugriff)
Für Ihren IP-Bereich sind aktuell keine Volltexte freigegeben.
Volltexte (frei zugänglich)
Es sind keine frei zugänglichen Volltexte in PuRe verfügbar
Ergänzendes Material (frei zugänglich)
Es sind keine frei zugänglichen Ergänzenden Materialien verfügbar
Zitation

Frey, M., Schneider, L., Razi, H., Trachsel, E., Faude, E., Koch, S. M., et al. (2021). High-performance all-bio-based laminates derived from delignified wood. ACS Sustainable Chemistry & Engineering, 9(29), 9638-9646. doi:10.1021/acssuschemeng.0c08373.


Zitierlink: https://hdl.handle.net/21.11116/0000-0008-EE23-5
Zusammenfassung
The need for renewable bio-based materials that could replace well-established synthetic composite materials is rapidly growing. For example, bio-based materials are increasingly used in applications where a lightweight design should be combined with sustainability and recyclability. However, it is often very challenging to directly transfer the excellent properties of biological materials to a product in a scalable and cost-efficient manner. In this study, we combined delignified wood layers (veneers) and a starch-based glue into bio-based high-performance composites. First, we investigated the ideal amount of starch-based glue between the layers to prevent delamination in the final composite. Then, we produced laminates in unidirectional, cross-ply, and quasi-isotropic configurations using wet processing. Laminates with tensile properties up to 40 GPa and 200 MPa in tensile stiffness and strength, respectively, were fabricated with a very high fiber volume content of up to 80. The high fiber volume contents led to mechanical interlocks between neighboring fibers and made the need for an additional matrix unnecessary. The water-based laminate process is cost-efficient and scalable and additionally allows one to make full use of delignified wood’s formability by producing shaped parts for various applications.